Hi All,

I am wondering if die attach with AuSn eutectic is used or if it is
necessary in the MEMS area. I understand that Au/Sn: 80/20 preforms are used
for die attach of stacked die where the reliability at higher temperature is
an issue.

We are developing a sputtering solution where we deposit a thick alloy of Au
and Sn in place of preforms. I will appreciate if anybody in the
mems-network could give suggestions or share their experience on this
aspect.

Thanks
Ravi Mullapudi
Hionix, Inc.
2157 O'Toole Avenue, Suite:E, San Jose, CA 95131
Phone: 408-910-8070  Fax:408-762-4305  www.hionix.com
----------------------------------------------------------------------------
----------------------------
The information contained in this e-mail message may be privileged,
confidential and protected from disclosure.  If you are not the intended

recipient, any dissemination, distribution or copying is strictly
prohibited.  If you think that you have received this e-mail in error,
please e-mail the sender at [email protected]

----------------------------------------------------------------------------
-----------------------------------




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.