MEMSnet Home: MEMS-Talk: SU-8 Chemical Resistance
SU-8 Chemical Resistance
2004-10-29
Srinivas Parimi
Leakage test
2004-10-31
rakesh babu
2004-11-01
Kirt Williams
EM simulation
2004-11-02
piyush tilloo
SU-8 Chemical Resistance
Srinivas Parimi
2004-10-29
Hello all,

I need to use SU-8 as a masking layer in R.T. KOH etching of silicon for
3-4 hours. Is this possible or would I have the same adhesion problems
associated with 70-90 C KOH etching ?

I also need to know how many hours SU-8 can resist 10 wt% HF. Is this also
a adhesion issue or will HF really attack SU-8 and if so, with what etch
rate?

Finally, Does anyone have a number on SU-8 electrical resistivity?

Thanks in advance

--
Srinivas Parimi
Research Assistant
Center for Microelectronics Sensors & MEMS  (CMSM)
372 ERC
University of Cincinnati
Cincinnati OH 45221
(513) 556 4795
Fax: (513) 556 7326
[email protected]
http://www.mems.uc.edu

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering