[email protected]
2004-11-03
Mark Fuller
optical adhesives
Mark Fuller
2004-11-03
At 07:44 AM 11/3/2004 -0700, you wrote:
>Dear all,
>
>I have been looking for a UV curable optical adhesive that will NOT cure
at all with a temperature increase to about 600 Celsius. Is this possible
to find? does anyone know about them?
>
>All the optical adhesive companies that I have contacted tell me that
their glues start reacting whith temperatures of around 60 to 100 celsius.
>
>Many thanks!
>
>anartz
>_______________________________________________

Is there any reason it must be UV cure?
Or that the adhesive must be applied before the 600C step?

--
Mark Fuller
Microelectronics Fabrication Facility
Washington State University
Dana Hall 102
Pullman, WA  99164-2711
(509)335-1797
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering