MEMSnet Home: MEMS-Talk: nickel etchants
nickel etchants
2004-11-05
Federico
2004-11-05
Shile
2004-11-08
Brent Garber
nickel etchants
Shile
2004-11-05
Aluminum Etch (Phosphoric acid based) works well for Ni.

Roger Shile

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Federico
Sent: Friday, November 05, 2004 7:39 AM
To: [email protected]
Subject: [mems-talk] nickel etchants

Hello everybody

anyone could suggest me an etchant for evaporated/sputtered/electoplated
nickel

thanks

Federico

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer