WALTER Harald
Is LPCVD oxide film really conformal
X. Yuan
2004-11-08
Hi,

I suppose the LPCVD oxide (950C) film is conformal.
But I just would like to know whether it is still
the case for a thin (500A) film deposition.
Especially, I want to know whether the vertical
side wall and the top of a structure (rectangular
cross-section) have the same thickness.
Or is there a way that I can measure the thickness
on the side wall? Thanks.

Yuan



__________________________________
Do you Yahoo!?
Check out the new Yahoo! Front Page.
www.yahoo.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
MEMS Technology Review
Harrick Plasma, Inc.