Wafer Thickness
2004-11-11
Craig Lowrie
2004-11-11
rakesh babu
2004-11-15
David Nemeth
2004-11-11
Jobert van Eisden
2004-11-15
Frank Torregrosa
2004-11-11
Pierre Huet
2004-12-07
Thilo Semperowitsch
Wafer Thickness
Pierre Huet
2004-11-11
Wafer back-grinding is a widely used process, feasible at most packaging
sites. Possible concerns (without knowing any specifics about your
project) about back-grinding:

- Mechanical pressure
- Contaminant from the chemicals used in the process
- Accuracy and uniformity of final thickness
- Texture required for the back-side

Regards,
Pierre x286
-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Craig Lowrie
Sent: November 11, 2004 09:32
To: [email protected]
Subject: [mems-talk] Wafer Thickness

Hello,

I am process restricted to using a 400 um thick silicon wafer but
require a thickness of 300 um.  Is there a possibility of using some
kind of post-processing "grinding" step or something similar to achieve
this? What would be the practical concerns of performing this if it is
possible?

Regards,
Craig
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer