MEMSnet Home: MEMS-Talk: RuO2 deposition
RuO2 deposition
2004-11-26
Philippe Combette
2004-11-27
[email protected]
RuO2 deposition
[email protected]
2004-11-27
Peeling of sputtered Ru is always a problem. Try capping it with some other
metal like W. Cleaning method will probably not help.
Niv



----- Original Message -----
From: Philippe Combette 
Date: Friday, November 26, 2004 12:02 pm
Subject: [mems-talk] RuO2 deposition

> Hi all,
> I have some difficulties in RuO2 films deposition by sputtering on
> different substrates like SiO2 and SiNx low stress. When the
> thickness is
> more than 120 nm, the film peel off on SiNx. I tried different
> clean
> methods (RCA, pirahna, with or without HF dip), but finally after
> few days,
> the films peel off. Is anyone got the same difficulties ?
> Thank you.
> Philippe Combette
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-
> talkHosted by the MEMS Exchange, providers of MEMS processing
> services.Visit us at http://www.memsnet.org/
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Nano-Master, Inc.