MEMSnet Home: MEMS-Talk: Adhesion promotor for Polypropylene
Adhesion promotor for Polypropylene
1998-03-11
Adhesivos Kefrén, S.A.
Adhesion promotor for Polypropylene
Adhesivos Kefrén, S.A.
1998-03-11
This is a multi-part message in MIME format.

------=_NextPart_000_0007_01BD4D25.0F613740
Content-Type: text/plain;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable

Dear MEMS discussion group members

I'm looking for a special polypropylene adhesion promotor (primer).

I need to bond it with a contact adhesive (polyurethane or polychloropre =
based).

Thanks in advance. If you know where I can find some information, please =
let me know.


Pablo Salvador
Director T=E9cnico

Adhesivos Kefr=E9n S.A.=20
 =20

------=_NextPart_000_0007_01BD4D25.0F613740
Content-Type: text/html;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable









Dear MEMS discussion group = members
 
I'm looking for a special = polypropylene adhesion=20 promotor (primer).
 
I need to bond it with a contact adhesive = (polyurethane or=20 polychloropre based).
 
Thanks in advance. If you know where I can find some = information, please let me know.
 
 
Pablo Salvador
Director Técnico
 
Adhesivos Kefrén S.A.
  
------=_NextPart_000_0007_01BD4D25.0F613740--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.
University Wafer