2004-12-08
Zhiyan Liu
Patterning of In coated surface
2004-12-09
li cai
Electrical conductivity
2005-01-13
Vikas Nair
Patterning of In coated surface
li cai
2004-12-09
Zhiyan,

Make PR thinner may help.

Li



>From: Zhiyan Liu 
>Reply-To: General MEMS discussion 
>To: [email protected]
>Subject: [mems-talk] Patterning of  In coated surface
>Date: Wed, 08 Dec 2004 11:26:12 -0700
>
>Dear friends
>
>I am wondering if anybody has experience on pattern In coated GaAs surface.
>I coated the GaAs surface with 1um of In, and then try to pattern it. I use
>the positive PR shipley 1818 and expose to UV light. But i can't get a
>sharp pattern, the edges are smear out. If anybody has suggestion, i really
>appreciate it.
>
>Thank you very much,
>Zhiyan
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
The Branford Group