Josef Kouba
2004-12-21
Hi Joe,

I have read a paper in Microelectronic Engineering (2004 - 73-74) about
direct writing of SU-8, what they reported was patternig of 280 nm thick
layer, pattern were cylinders with a diameter of 100 nm. check the paper.

regards

J.


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of laetitia philippe
Sent: Dienstag, 21. Dezember 2004 12:25
To: [email protected]
Subject: [mems-talk] EBL + SU8


Hello Al,

I wonder if SU8 is a good candidate for ebeam lithography since I know below
350 nm, it behaviour can be difficult. Also, has someone try to see the
resolution obtained with EBL and SU8

Is it possible to make successive exposition-developpement on a thick layer
of SU8, in order to pattern higher aspect rations, if a good resolution
table permits to positionate the sample exactly at the same place?

many thanks
Joe


---------------------------------
 Découvrez le nouveau Yahoo! Mail : 250 Mo d'espace de stockage pour
vos mails ! Créez votre Yahoo! Mail
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us
at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
University Wafer
Nano-Master, Inc.