I am looking for a foundry that can place a patterned metal of at least
100µm thickness onto a 4-inch wafer.  Some options for this would be direct
electroplating, or bonding patterned metal to the wafer.  The pattern would
be a grid of 170µm holes on 340µm pitch.  Metals can be gold or molybdenum
or anything with a reasonable thermal match to GaAs.

Any assistance would be greatly appreciated.

Brad Cantos
Dir. Wafer and Die Operations
Novalux, Inc.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer