MEMSnet Home: MEMS-Talk: Peel Off
Peel Off
2005-01-05
Z.,W.Y.(Lydia)
2005-01-05
Kasman , Elina
Peel Off
Z.,W.Y.(Lydia)
2005-01-05
Dear All,

When I etched my wafers using buffer HF(NH4F: HF=10:1), Sio2 was etched away,
however, lots of pink pieces dropped into solution. After DI water resining and
spinning dry, more and more pink pieces appeared and stuck to the wafer. And
large areas in wafer-frontside(suppose to be PR) looked uniformly, i.e. some
area look darker than others. The backside sio2 removed compeletely.

I processed those wafers using the following step:
1) RCA clean silicon wafer and Wet-oxidize (~1 um)
2) O2 plasma etch the front side (for cleaning) [2 min, 300W, 300 mtorr]
3) Photolithagraphy (130C/1hr dehydration bake, 10 min HDMS vaper prime,
spin-coat PR[OCG825], 95C/30min softbake, exposure, develop, 130C/30min hard
bake)
4) BHF etch SiO2 for 17 min and DI risine and spin dry. (backside SiO2 has been
etched away since no protection)

Are those pink pieces PR or SiO2? Any suggestions for possible reasons or
improvements are highly apperaciate.

Lydia

-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics