MEMSnet Home: MEMS-Talk: Ti and Cr resistivity
Ti and Cr resistivity
2005-01-05
Imran Ghauri
2005-01-05
Kirt Williams
2005-01-06
MT Klaus Beschorner
2005-01-07
Damiano Galvan
2005-01-07
MT Klaus Beschorner
Ti and Cr resistivity
MT Klaus Beschorner
2005-01-06
> I'm looking for Ti thin film resistiivty and Cr thin
> film resistivity. Resistivity vs. temp. data of these
> thin films will also be appreciated.

Both materials are highly reactive, so resistivity will strongly
depend on base vacuum/leakup rate of the deposition equipment.
And, I mean, REALLY STRONGLY depend!

For our PVD equipment, we spec:
Ti <65 micro-Ohm-cm at 300 C
Cr <35 micro-Ohm-cm at 300 C
actual values are usually ca. 10% lower.

The higher the temperature, the lower the resistivity, under
clean conditions. This is often masked by increased out-gassing
of chamber parts at higher temperature.

best regards,
klaus

--
Klaus Beschorner
Metron Technology, European Applications Manager
Drosselweg 6,71120 Grafenau,Germany. Tel +49-7033-45683

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Mentor Graphics Corporation