MEMSnet Home: MEMS-Talk: TaN
TaN
2005-01-11
Mojgan Daneshmand
2005-01-11
Neal Ricks
2005-01-12
Mahavir Sanghavi
2005-01-12
Mojgan Daneshmand
2005-01-12
Neal Ricks
Re:TaN
2005-01-14
Damiano Galvan
TaN
Mojgan Daneshmand
2005-01-11
Hi everyone,
I am trying to deposit a resistor layer and I thought using TaN would be
a good idea. Has anyone deposited TaN before using any technique? If
yes, was that sputtering or evaporation? I believe sputtering target is
expensive, would it help if I go toward evaporation? Is there any
concern that I should take it in to account?

I would really appreciate your answers.
Thanks in advance
Mojgan



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review