Li Wang
2005-01-11
Isaac Wing Tak Chan
2005-01-12
Oliver Horn
2005-01-11
Kory Hall
lift-off
Oliver Horn
2005-01-12
Hi,

did you measure the temperature or the bias-voltage during deposition?
In my experience Ni gets a very high bias-voltage, up to 2000 V. This
leads to a high temperature on your substrate, which would harden the
photoresist.

Perhaps you could try less power or substrate movement to keep it cool.

Best regards,

Oliver Horn

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics