Asking help on Cu etchants
Jun Zou
1998-03-20
Hi,

Now we are developing a structure, using Ni(structural layer) and Cu
(sacrificial layer). We want to find a good etchant for Cu, but not
attacking Ni or permalloy.

So could anyone give me some information about that?

Thanks a lot!

Jun Zou


--------------------------
Jun Zou
209 E.Clark Street Apt#2
Champaign, IL 61820
USA
Tel:(217)-265-0808(O) (217)-351-7448(H)
E-mail: [email protected]
--------------------------


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing