RE: polymers for intermediate wafer bonding
2005-01-17
Zoberbier, Margarete
2005-01-17
Shile
RE: polymers for intermediate wafer bonding
Zoberbier, Margarete
2005-01-17
Dear Brijesh,

there are diffirent polymers / adhesives which can be used as an
intermediate layer for bonding purposes. The following samples gives an
overview about the material range: Epoxies, UV-Epoxies, positiv / negativ
photoresist, BCB, PMMA, PEEK, thermosetting coplyesters, PMDS, Polyimides
and Waxes. Practically all types of wafer materials can be joined with
adhesive bonding. The exact bonding procedure depends on the adhesive
material.

A good overview about different adhesive bonding processes gives the
following paper
Low-temperature full wafer adhesive bonding,
by Frank Niklaus, Peter Enoksson, Edvard Kälvesten and Göran Stemme
http://www.iop.org/EJ/abstract/0960-1317/11/2/303

Best Regards,
Margarete Zoberbier

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer