MEMSnet Home: MEMS-Talk: Thick film resist, 320nm absorbance
Thick film resist, 320nm absorbance
2005-01-17
George Lopez Subrebost
Thick film resist, 320nm absorbance
George Lopez Subrebost
2005-01-17
MEMS talk colleagues:
        Is there a thick film photoresist (>10 microns) that can be exposed with
a
320nm wavelength?  AZ4600 series resist is geared for absorption in g, h,
and i-line (>320nm).
        Thanks,
                George