su-8 ahesion
Sonia Garcia Blanco
2005-01-18
Hi Liu,

You can also spin a layer of adhesion promoter APS300 from Silicon Resources
before spinning the SU8. It worked for me.

Also, be extremely careful with the baking steps, specially the post
exposure bake, as if you cool down the samples too quickly the stresses
generated can produce peeling of the structures.....

Good luck!

Sonia.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Harrick Plasma, Inc.
Nano-Master, Inc.