MEMSnet Home: MEMS-Talk: plasma-etching of fused silica
plasma-etching of fused silica
2005-01-17
Marlene
2005-01-17
Parijat Bhatnagar
2005-01-18
Marlene Brod
2005-01-18
Kirt Williams
2005-01-18
[email protected]
plasma-etching of fused silica
Kirt Williams
2005-01-18
See "Etch Rates for Micromachining Processing-Part II," Journal of
Microelectromechanical Systems, vol. 12, no. 6, Dec. 2003, pp. 761-778,
online at
http://microlab.berkeley.edu/labmanual/chap1/JMEMSEtchRates2(2003).pdf  .
Note the fused silica is the same as fused quartz.
    --Kirt Williams

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing