A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Mask for H2O2
Mask for H2O2
2005-01-21
Tomi Meilahti
Mask for H2O2
Tomi Meilahti
2005-01-21
Hi folks
I´m looking for a mask material to be used in wet etching of tungsten in a
30% solution of H2O2 or in a solution consisting of H2O2/NH4OH/DIW. I´m
espesially interested in a H2O2 resistant material. Tungsten foil used is 25
microns thick and it is etched through in about 2 hours. Material should be
as easily appliable, patternable and strippable as possible. I tried thin
layers (150nm) of Al and AlN but those didn´t work. They lasted under 30
seconds. Any ideas would be greatly appreciated.
Tomi Meilahti
Oxford Instruments Analytical Oy
E-mail: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group