MEMSnet Home: MEMS-Talk: wet etch of SiO2 or SiC selective to NiSi/CoSi2
wet etch of SiO2 or SiC selective to NiSi/CoSi2
2005-01-27
[email protected]
wet etch of SiO2 or SiC selective to NiSi/CoSi2
[email protected]
2005-01-27
Hello,

Did you find a solution to etch SiO2 without etching NiSi?
I tried buffered HF but it didn't work.

Yours sincerely
Michael Grieb