MEMSnet Home: MEMS-Talk: anti stiction coating
anti stiction coating
2005-01-28
Amani Salim
2005-01-28
Jim Beall
deposit TaN for Cu barrier
2005-01-30
li cai
2005-01-29
Natalya
anti stiction coating
Natalya
2005-01-29
 Hi Amani,

Self-assembled monolayers (SAMs)are widely used as an anti-stiction coating
for MEMS, microcontact printing and other applications. Applied
Microstructures manufactures a tool for SAMs deposition in a vapor phase.
We also developed some special techniques to make release layers more
durable. You may contact me for further information and arrange some
demonstration experiments.

Boris Kobrin
(408) 594-0654
[email protected]
www.appliedmst.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering