MEMSnet Home: MEMS-Talk: RIE metal etching
RIE metal etching
2005-02-02
fabio quaranta
2005-02-02
Brent Garber
2005-02-02
Shile
2005-02-03
Kirt Williams
2005-02-02
[email protected]
RIE metal etching
[email protected]
2005-02-02
I would use TiW which meets your needs as far as etching goes. Bob Henderson

reply