MEMSnet Home: MEMS-Talk: Photoresist
Photoresist
2005-02-09
Guiti Zolfagharkhani
2005-02-10
Tushar Bansal
2005-02-10
Karin Buchholz
2005-02-10
Kory Hall
2005-02-10
Behraad Bahreyni
Photoresist
Behraad Bahreyni
2005-02-10
I have used HPR504 to etch ~10um of silicon in a DRIE system (the
photoresist polymerized and had to be removed by piranha) and HPR506 to
etch ~20um of silicon in an RIE system with no problem.

Behraad

reply