Hi folks

Does anyone have a good recipe for tungsten wet etching? What we are trying
to do is etch through a 25um tungsten foil. At the moment we are using 30%
H2O2 in 50C temperature and that does the job in about  two hours. The only
problem is finding a suitable, patternable and preferably easily strippable
masking material for this process. Any suggestions or ideas are highly
appreciated.

Tomi Meilahti
[email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
MEMS Technology Review
Mentor Graphics Corporation