Bonding SU-8 to polyimide
2005-02-17
김종호
2005-02-17
Bill Moffat
Bonding SU-8 to polyimide
Bill Moffat
2005-02-17
Jongho,
       Early adhesion methods for Polymide used AminoPropylTriEthoxySilane,
APTES.  It worked so well the Polymide manufacturers incorporated it into the
liquid Polymide.  The old method of using it was to mix it with water and spray
or spin it on.  I have a vapor deposition system that puts sown vapor APTES and
other silanes.  If it is practical I can put down a vapor APTES coating for you.
Bill Moffat

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation