dryetch Al selectiv to Si
2005-02-17
Bill Moffat
2005-02-19
[email protected]
dryetch Al selectiv to Si
[email protected]
2005-02-19
Sorry; the chlorine chemistry used for etching aluminum also etches silicon .
Bob Henderson