MEMSnet Home: MEMS-Talk: Mechanical characterization of thin films
Mechanical characterization of thin films
2005-02-20
harshal rokade
2005-02-20
mahdi bagheri
2005-02-22
harshal rokade
Residual Stree In Thin Film
2005-02-20
singh
2005-02-20
Mark da Silva
2005-02-21
Josef Kouba
2005-02-22
harshal rokade
2005-02-26
Nikhil Mehta
2005-02-21
sampath kumar paduru
Mechanical characterization of thin films
Mark da Silva
2005-02-20
Hi Harshal

You may be interested in the standardisation work for Mems/MST thin
films available through ASTM (
http://www.astm.org/cgi-
bin/SoftCart.exe/DATABASE.CART/REDLINE_PAGES/E2244.htm?E+mystore

there is more recent work done on elastic moduli but it's not available
just yet.

Mark

harshal rokade wrote:

>Which is best way to find out mechanical properties of thin fims.
>also how to find the properties such as stiffnes, Young's Modulus
>of cantilevers made of thin films..

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group