MEMSnet Home: MEMS-Talk: Etchant for SiO2 without etching Aluminum
Etchant for SiO2 without etching Aluminum
2005-02-18
Ramesh Narayanan
2005-02-21
Ramesh Narayanan
2005-02-22
ZICKAR Michaƫl
Etchant for SiO2 without etching Aluminum
Ramesh Narayanan
2005-02-21
Hi,
I  have deposited aluminum on SiO2(wafer). I have etched the aluminum
leaving finally a SiO2 and small square of aluminum pattern, could you
please suggest me an etchant which can etch SiO2 with out etching
Aluminum and also could you please suggest whether I could Photo resit
as the mask to etch SiO2?.
Thanks
Ramesh

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics