Re: solubility of PMMA
2005-02-23
Harald Walter
2005-02-23
[email protected]
Re: solubility of PMMA
[email protected]
2005-02-23
thanks for your answer.
I want to use PMMA as a mask .
I tried to put wafer with PMMA coating(300nm) in methannol for around 12 hours,
at lease it looks like  still OK,
what do you mean methanol is bad for the stable of PMMA?

thanks

best

Yu Chen