MEMSnet Home: MEMS-Talk: Fabricate Silicon cantilevers
Fabricate Silicon cantilevers
2005-02-24
Kevin Duan
2005-02-24
Shile
Fabricate Silicon cantilevers
Kevin Duan
2005-02-24
Hi Dear all,

I am trying to make cantilevers that can be used in AFM(Atomic Force
Microscope), and silicon cantilever is one of my object.  Using SOI
wafer is the mostly common and simple way to achieve that, however,
the expense is high.  Does someone know any other method to fabricate
silicon cantilevers?  Any related papers?  It will be very kind of you
to help me.

Best regards.

Duan

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review