A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: wire bonding gold wire to platinum pads
wire bonding gold wire to platinum pads
2005-02-24
Jesse D Fowler
2005-02-25
Michael D Martin
wire bonding gold wire to platinum pads
Jesse D Fowler
2005-02-24
Hi everybody,
I'm trying to wire-bond to Pt pads using Au wire.  I'm using an ancient West-
bond wedge bonder, the wire is, I believe, 30 um diameter, and currently I'm
having luck doing the termination bonds using medium power for a long time. I
have the package at 350
C, and I think the chip surface is about 280.

I was wondering if anyone out there has some advice on how to do a starting
bond, and how to zero in on better quality bonds.

Also, I'm looking for a wire-bonding service in the Los Angeles area for a batch
of about 50 chips with 20 wires per chip (~2000 bonds).

I looked through the list about a month ago, with sparse information presenting
itself.

Thanks,
Jesse Fowler


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics