MEMSnet Home: MEMS-Talk: etching fine (hundreds of nanometers) features on metal?
etching fine (hundreds of nanometers) features on metal?
2005-02-28
Daniel Lloyd
TiN and TaN
2005-03-01
li cai
2005-03-01
Qinghong Du
2005-03-02
Suhua Jiang
etching fine (hundreds of nanometers) features on metal?
Daniel Lloyd
2005-02-28
Hi,

We've made structures of this sort using photo-lithographic techniques
on silicon and then RIE into substrates. Coating them with gold has
worked well for laser diffraction gratings, but this can be an expensive
process unless you have the equipment.

Daniel Lloyd
Assistant Development Engineer
Laser Optical Engineering Ltd

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.