David Springer
2005-03-02
Hi Ramesh

If you would prefer a dry release etch for your cantilevers you might want to
consider using xenon difluoride (XeF2) gas to etch away the silicon under your
cantilevers. XeF2 has very high selectivity to almost all materials including
most metals.

If you would like to discuss this more or try it out please contact me.

Regards
David Springer
XACTIX, Inc.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering
MEMS Technology Review