MEMSnet Home: MEMS-Talk: AZ4620 Removal after High temperature Bake
AZ4620 Removal after High temperature Bake
2005-03-09
Michael
2005-03-10
Kasman , Elina
2005-03-11
CY Hsieh 謝吉勇
2005-03-14
Russell Davies
AZ4620 Removal after High temperature Bake
Kasman , Elina
2005-03-10
Try AZ Kwik Strip - it's designed for AZ4620.
But after baking at this high temperature, I doubt you will be
successful...