Si/Au Ohmic Contact
Eric J. Correa
2005-03-11
Hello Everyone:

I am trying to make an ohmic contact between gold and
silicon to perform some electrical measurements.  I would
like to know the annealing temperature to create an ohmic
contact between Si/Au.  Any recommendation for this process
will be also helpful.

Thanks in advance;

Eric J. Correa Rivera
Graduate Student
Mechanical Engineering
University of Illinois at Urbana Champaign

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group