Dear All:
   I need a 5um or thicker photoresist pattern.since 1827 can give 3um thick, I
plan to double coat . the smallest linewidth is 3um, How the expose and
development time change? Could you give me some suggestions on how to produce
5um positive PR ? than you very much.
Jason
[email protected]
716-5872761
Pennstate University


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer