MEMSnet Home: MEMS-Talk: PDMS thickness variation with spin speed and time.
PDMS thickness variation with spin speed and time.
2005-03-15
Kapil Sahasrabudhe
2005-03-15
[email protected]
2005-03-15
Gary
2005-03-15
[email protected]
2005-03-16
[email protected]
2005-03-16
[email protected]
2005-03-16
[email protected]
2005-03-16
Kapil Sahasrabudhe
2005-03-15
Z.,W.Y.(Lydia)
2005-03-16
karim faid
2005-03-17
Z.,W.Y.(Lydia)
PDMS thickness variation with spin speed and time.
[email protected]
2005-03-16
Hi Joe

What are some of the application that you can use SU-8 for..?

Cheers
Mr. Arie Ross

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.