MEMSnet Home: MEMS-Talk: RE: Spam:[mems-talk] coating a teflon layer on 8um glass spheres
RE: Spam:[mems-talk] coating a teflon layer on 8um glass spheres
2005-03-17
Matthew Coda
RE: Spam:[mems-talk] coating a teflon layer on 8um glass spheres
Matthew Coda
2005-03-17
I would use a reactive monolayer approach.  Consider a ethoxysilane
terminated medium length fluorinated alkyl chain (maybe 20 units).
Apply in solution.  As a cheap first pass try octadecyltriethoxysilane
(I believe you can purchase this from Aldrich), it's not fluorinated but
it'll give you a nice hydrophobic surface on the glass.

-Matt

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.