how to prevent the natural oxide formation on poly-Si film for transportation?
2005-03-20
X.Guo
how to prevent the natural oxide formation on poly-Sifilm for tr
2005-03-21
li cai
how to prevent the natural oxide formation onpoly-Sifilmfor tr
2005-03-21
Jesse D Fowler
how to prevent the natural oxide formation onpoly-Sifilmfor tr
Jesse D Fowler
2005-03-21
Assuming that "ultra-thin" means you can't expose it to liquids, you can pack it
in a dry box environment (a nitrogen filled glove box) in some sort of sealed
container. Personally, I would use a mason jar, but there's probably something
much better
("more expensive") to use for that sort of transport.

Jesse Fowler




             "li cai" 
             Sent by: [email protected]
            To
                               [email protected]
             03/20/2005 05:41 PM
cc

       Subject
                                                 Please respond to
RE: [mems-talk] how to prevent the natural oxide formation onpoly-Sifilm for tr
                                  General MEMS discussion 









How thin is the film?  Dip in DILUTED HF may help.

>I have a sample with ultra-thin poly-Si film on the top to be transported.
>Does anybody know any ways to prevent the formation of the natural oxide
>layer on the poly-Si film during transportation?
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Nano-Master, Inc.