A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: polishing the DRIE scalloping
polishing the DRIE scalloping
2005-03-18
Rahul Agarwal
2005-03-21
Eric Dy
polishing the DRIE scalloping
Eric Dy
2005-03-21
You can try using hydrogen annealing if your lab has the capabilities.

Lee, Ming-Chang, "silicon profile transformation and sidewall roughness
reduction using hydrogen annealing"

Eric

reply