Dear All,
   A layer of Ti was deposited on substrate by e-beam.
But I can not make pattern on it by HCl. Is there an
oxidation layer on Ti film which protects it? If so,
how long does it take to form an oxidation layer after
the film exposed to the air? And how to remove this
layer by wet or dry etching? Thanks a lot!

ZHU X P

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group