Problem in photolithography
2005-04-01
[email protected]
2005-04-01
Kamat Mahesh Keshav
2005-04-01
Haroon Lais
2005-04-01
Brubaker Chad
2005-04-02
Mahesh Pitchumani
Problem in photolithography
Brubaker Chad
2005-04-01
I would actually be more likely to look at my exposure to begin with.

There is a wide variety of photolithographic materials out there, ranging from
ultra-thin (<100nm) to ultra-thick (>100 μm), and the process parameters will
depend on which material you are using.

Which photoresist are you processing with, to what thickness, and what is your
exposure process (dose, lamp intensity).

Best Regards,
Chad Brubaker

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group