MEMSnet Home: MEMS-Talk: PDMS shrinkage problem
PDMS shrinkage problem
2005-04-07
[email protected]
2005-04-07
Jim Beall
PDMS shrinkage problem
[email protected]
2005-04-07
Hi, everyone,
     I am facing an alignment problem associated with PDMS shrinkage.
I was trying to align and seal a PDMS slab on a glass slide. But I
found PDMS slab had a size change up to several percentage, after
peeled off from SU8 mold.
     This made it impossible to well align the slab on glass slide.
(There are microfabricated patterns on the glass slide). Does anyone
have this problem before? How would you solve the problem?
     I feel that I may have seen this problem reported somewhere, but
cannot find the publication now. Please help me out, thank you very
much. Any suggestions will be appreciated.

--
Best Regards,
Shawn

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review