MEMSnet Home: MEMS-Talk: Ni etching on GaAs substrate
Ni etching on GaAs substrate
2005-04-12
X.P. Zhu
2005-04-12
Brent Garber
2005-04-12
[email protected]
Ni etching on GaAs substrate
X.P. Zhu
2005-04-12
Dear members,
   I want to pattern Ni film on GaAs substrate by wet
etching. The one micron thick film was deposited by
E-beam. I used diluted HCl and H2SO4 and they did
work, but H2 bubbles generated during the etching
procedure made effect on the etching uniformity: they
all attached to the wafer surface. How to do with
these bubble? Or are there any other etchants which
can etch Ni but not GaAs, and don't release bubbles
during etching? Thanks!

ZHU X.P.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics