MEMSnet Home: MEMS-Talk: Spin-On -- Lift-Off SOLO?
Spin-On -- Lift-Off SOLO?
2005-04-13
Avi Laker
2005-04-13
[email protected]
Spin-On -- Lift-Off SOLO?
Avi Laker
2005-04-13
anyone ever done a lift-off with a spin on material where the
spin on material is what you would like to keep?
ie, use 20 microns of resist  as a mask for a
10 micron spin on glass?

thanks


reply