how to do edge bead removal by hand?
2005-04-12
Jiang Ziling
2005-04-13
Isaac Wing Tak Chan
polish
2005-04-13
Hongjun-ECE
2005-04-12
Jobert van Eisden
2005-04-12
Kory Hall
2005-04-14
Vladimer Michael
polish
Hongjun-ECE
2005-04-13
Dear colleagues,

I'm going to polish a copper surface. We have a polisher but don't know how
to get a mirror like surface. Do you know:

1. How much is the size of powder/sheet can get mirror like polishing? Any
type? Al2O3 or something else?
2. I remember some liquid should be added during the polishing. What is that
liquid? Water? Is the liquid only for lubrication?

Thanks for your help,

Hongjun

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.