hi all,

  I tried to make channel by bonding two Glass wafers, one with a 50um
exposed Su-8 layer with channel on it, another with a 50um unexposed
Su-8 layer. According to some research, at 75 degree centigrade the
unexposed Su-8 can reform shape and bond with the exposed layer when
certain pressure is applied. But I tested and found that the 100um
wide channels on the exposed su-8 surface are always clogged by the
soft Su-8 flowing from the unexposed layer during pressing-bonding.
However, if I don't press, there will be no bonding. Does anyone have
experience in solving this clogging problem?

 best regards

 Jiang Ziling
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.
Nano-Master, Inc.