MEMSnet Home: MEMS-Talk: back-side etch: uniform temperature
back-side etch: uniform temperature
2005-04-19
[email protected]
2005-04-20
Shay Kaplan
2005-04-19
Liwei Wang
2005-04-20
Joe Lonjin
2005-04-20
[email protected]
back-side etch: uniform temperature
Liwei Wang
2005-04-19
Hi, Elena

You can use a larger water bath to put your TMAH container in and heat
up the whole bath, that will give you a very uniform temperature
control.

Liwei

>>> [email protected] 04/19/05 1:41 PM >>>
Does any one know of heaters (say a ceramic plate that is
submerged vertically in solution) that provide uniform
temperature throughout the etching solution? I am doing a
back side etch on an 8'' wafer, using a very large container
filled with TMAH, but the wafer etches differently at the
bottom and at the top.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering
The Branford Group